VisualizationTiered Utensil Station SVG, Buffet Cutlery Holder Laser Cut File, Three Step Flatware Display Stand DXF
A tall three-step stand that presents cutlery upright on the counter or a buffet, with four slots on every step for 12 compartments in total. It measures 320 × 320 × 240 mm (12.60 × 12.60 × 9.45 in), is cut from 18 plywood pieces that slot together with tabs, has small part numbers engraved on the pieces to guide assembly, and is a free SVG and DXF download with separate files for 3, 4, 5 and 6 mm plywood.
- Formats
- SVG, DXF
- Outer size (W × D × H)
- 320 × 320 × 240 mm (12.60 × 12.60 × 9.45 in)
- Parts
- 18
- Material thickness
- 3, 4, 5 or 6 mm plywood (a file for each)
- Layout size (3 mm file)
- 1,346 × 447 mm
- Cut length
- 13.82 m
- Est. time, 10 W diode (3 mm)
- 46 min 04 s
- Est. time, 40 W CO2 (3 mm)
- 19 min 12 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Choose the file for your sheet thickness and cut a single divider and shelf corner to check that the slot fit is snug.
- 02Cut all 18 numbered pieces, spreading the two tall side panels over separate sheets if your bed is short.
- 03Seat the three shelves, the step boards and the back brace between the two side panels, then press the nine dividers into their slots.
- 04Sand the shelf edges, coat the stand with a wipe-on lacquer and fill each step with forks, spoons, knives and chopsticks.
A self-serve station for twelve kinds of cutlery
Three shelves rise toward the back, each one higher than the step in front, and three dividers on every shelf create four slots across. The photo repeats the same order on each level: forks on the left, then spoons, butter knives and a bundle of wooden chopsticks on the right, so guests find what they need on whichever step is closest. At 240 mm tall the back row lifts handles well above the counter, where they are easy to spot from across a table, which is why this version suits a buffet, a staff room or a cafe pickup shelf better than a drawer.
The footprint is a square 320 × 320 mm, so it fits a corner of a kitchen island without taking over the worktop.
Putting the steps together
There are 18 pieces: two stepped side panels, a front board, two step boards, three shelves, a brace that stiffens the back and nine dividers. One shelf is a little deeper than the other two and takes the three longer dividers. Small part numbers are engraved on every piece, so lay them out in order before you start. Fit both sides onto the shelves first, add the step boards and the brace, and finish with the dividers.
The 3 mm sheet is 1346 × 447 mm and the cut line totals 13818 mm. For the 3 mm file allow about 46 min 04 s on a 10 W diode, about 19 min 12 s on a 40 W CO2 or about 9 min 13 s on a 100 W CO2. On a small bed, split the side panels and shelves across two or three sheets.
For events and small cafes
- Engrave your cafe logo on the front board yourself and use it at the coffee counter.
- Rent it out with wedding buffet decor alongside matching napkin boxes.
- Sell it to office kitchens as a tidy shared cutlery station.
Questions about this file
How many pieces of cutlery does each slot take?
Each slot comfortably holds a handful of forks or spoons standing upright. For a buffet of about 20 guests, one slot per type on each step is usually enough.
What do the engraved numbers on the pieces mean?
They are small part numbers that tell you which shelf, step board or divider goes where. They are the only engraving in the file and can be sanded off after assembly.
Can I scale this stand down for a smaller counter?
You can, but keep the slot width equal to your plywood thickness after scaling or the joints will be loose. Scaling by 80% gives a stand about 192 mm tall.
Is 3 mm plywood strong enough for a stand this tall?
Yes for cutlery, because the brace and step boards tie the sides together. Use 4 or 5 mm if it will be moved around full at events.
How do I keep it clean at a busy buffet?
Seal it with a water-resistant lacquer so it can be wiped down. Leave the dividers unglued if you want to lift them out and wash around them.
Similar files