VisualizationBook Style Tea Box SVG, Living Hinge Tea Gift Box Laser Cut File, Wooden Book Box DXF, Kerf Bend Tea Case
A free book-style tea box laser cut file in SVG and DXF, with separate versions for 3, 4, 5 and 6 mm plywood. It measures 400 × 180 × 90 mm (15.75 × 7.09 × 3.54 in) and is cut as 7 pieces that join with tabs and slots. Its one-piece cover wraps over the box like a book cover on a flexible spine of thin kerf cuts, and the inside is a single open compartment.
- Formats
- SVG, DXF
- Outer size (W × D × H)
- 400 × 180 × 90 mm (15.75 × 7.09 × 3.54 in)
- Parts
- 7
- Material thickness
- 3, 4, 5 or 6 mm plywood (a file for each)
- Layout size (3 mm file)
- 2,055 × 188 mm
- Cut length
- 16.99 m
- Est. time, 10 W diode (3 mm)
- 56 min 39 s
- Est. time, 40 W CO2 (3 mm)
- 23 min 36 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Download the 3 mm version unless you have a reason to go thicker, and test-bend a small kerf sample cut from the same sheet.
- 02Cut the 7 pieces on a bed long enough for the 847 mm cover, keeping the plywood perfectly flat while the kerf section cuts.
- 03Join the front, back and two long sides, then wrap the cover slowly around them, easing the flex spine into its curve and seating its tabs.
- 04Sand lightly, finish everything except the bending area with a thin coat, and fill the compartment with tea.
One room inside, a cover that bends
The box itself is a front, a back and two long sides. The cover is one long panel: part of it is cut with rows of thin kerf lines, and that section bends into a rounded spine, so the same panel wraps around the box like a hardback book. A small pin piece completes the set. Inside there is one open compartment, 400 mm long. The photo shows it fitted with a long strip and three short ones to make two rows of four, with tins of loose tea at the back and tea bags in front. Those dividers are not in the file: cut them from plywood strips a little lower than the walls if you want the same layout.
Getting a clean flex spine
The living hinge bends best in good-quality birch plywood with no voids; cheap poplar or MDF tends to crack along the kerf lines. Bend the spine slowly, a little warmth from a hair dryer helps, and never force it past the shape of the box. Keep thick lacquer off the kerf section so it stays flexible.
All those kerf lines make this a longer job than most tea boxes: about 56 min 39 s on a 10 W diode, about 23 min 36 s on a 40 W CO2 and about 11 min 20 s on a 100 W CO2, all for the 3 mm file. The cover is a single piece about 847 mm long, so you need a bed at least that long or a machine with a pass-through slot; the full layout is 2055 × 188 mm. Thicker plywood makes the spine much stiffer, so 3 mm is the easiest version to bend.
A tea gift that looks like a book
Fill it with a tea collection and it reads as a gift before it is opened. Engrave a title on the front cover, such as a name and a year, to turn it into a keepsake for a bookshelf. It also suits a tea ceremony set or a stack of herbal sachets.
Questions about this file
How does the spine bend without a hinge?
It is a living hinge: rows of thin kerf cuts let solid plywood flex, so no hinge hardware is needed.
Which plywood bends without cracking?
Void-free birch plywood in 3 mm bends most smoothly. Poplar, cheap laminated sheets and MDF often snap along the cuts.
Are dividers included like in the photo?
No, the file is one open compartment. Add your own strips from scrap if you want rows for tins and tea bags.
My laser bed is only 400 mm long. Can I still make the book box?
The cover is one piece about 847 mm long, so it needs a longer bed or a pass-through slot; cutting it in parts would lose the flex spine.
Can I personalise the cover?
Yes, add an engraving layer with a name, title or pattern on the front cover in your design software before cutting.