VisualizationBass Fishing Key Rack DXF, Fisherman Coat Hook Hanger SVG, Leaping Bass Wall Hooks, Plasma Cut Fishing Decor
A fishing-themed wall hook rack: a largemouth-style bass leaps out of the water at a lure, while a small fisherman casts from a dock among reeds, all inside an oval frame on a bar with two screw holes and four flat prongs. The free SVG and DXF contain cut lines only, 245.4 × 167.2 mm (9.66 × 6.58 in), drawn for metal, where the prongs bend up into hooks.
- Formats
- SVG, DXF
- Size
- 245 × 167 mm (9.66 × 6.58 in)
- Material
- Plywood, MDF, acrylic or metal (scale to your piece)
- Cut length
- 4.49 m
- Est. time, 10 W diode (3 mm)
- 14 min 59 s
- Est. time, 40 W CO2 (3 mm)
- 6 min 14 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Delete the stray dot and decide on metal hooks or a wooden version with added pegs.
- 02Cut the oval scene, bar and prongs, starting with the inner slots of the bass.
- 03Bend the steel prongs forward and curl the tips, or fit hooks or dowels to a wooden bar.
- 04Paint or powder coat the rack and screw it to the wall through the two holes in the bar.
The scene
The bass fills the left half of the oval with its mouth wide open, gill lines, fin rays and a spotted belly picked out as small slots. The fishing line runs from the lure in its mouth up to the rod of a fisherman standing on a dock at the right, with reeds and a splash of water around them. Everything is joined to the oval, which sits on a straight bar with two screw holes. Four long, round-tipped prongs hang from the bar.
Metal or wood
In 2–3 mm steel cut on a plasma table or fibre laser, bend each prong forward and curl the tip up, and you get four sturdy hooks like the black powder-coated rack in the photo. In plywood or acrylic the prongs cannot bend, so trim them off in your software and screw four small coat hooks or wooden pegs to the bar instead, or glue on short dowels angled upward. The fin and belly slots are narrow, so for wood keep the rack at the drawn size or larger.
One tiny stray dot sits off to the right of the drawing; delete it before cutting.
Where to hang it
By the back door for keys, caps and a landing net, in a cabin hallway for jackets, or in a boat garage for waders and lanyards. It is an easy gift for anglers on Father's Day or a retirement, and it pairs well with a fishing sign or a tackle box. Engrave a lake name or a family name on the bar if you add a wider strip.
Questions about this file
How do the hooks work?
The four prongs are flat in the file. In steel, bend them forward and curl the tips to make hooks.
Can I cut it in wood?
Yes, but wood cannot bend, so remove the prongs and screw on metal hooks or glue in dowel pegs.
What is the small dot to the right?
A stray mark in the drawing. Delete it before sending the file to your machine.
Which steel thickness is best?
About 2–3 mm mild steel bends by hand in a vice and still holds coats and keys.
Can I scale it up?
Yes, a 400 mm version holds heavier coats; scale the screw holes back to your screw size.