VisualizationWraparound Cover Spice Box SVG, Cookbook Style Spice Chest DXF, Flex Spine Seasoning Box Laser Cut File
A free laser cut file for a book-shaped spice box: one long cover panel with a flexible living-hinge spine of thin kerf cuts wraps around the box and closes over the top like a book cover. It measures 280 × 220 × 100 mm (11.02 × 8.66 × 3.94 in), has one open compartment, is cut from 7 plywood pieces, and includes SVG and DXF files for 3, 4, 5 and 6 mm plywood.
- Formats
- SVG, DXF
- Outer size (W × D × H)
- 280 × 220 × 100 mm (11.02 × 8.66 × 3.94 in)
- Parts
- 7
- Material thickness
- 3, 4, 5 or 6 mm plywood (a file for each)
- Layout size (3 mm file)
- 1,661 × 228 mm
- Cut length
- 19.97 m
- Est. time, 10 W diode (3 mm)
- 66 min 35 s
- Est. time, 40 W CO2 (3 mm)
- 27 min 44 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Choose the thickness folder and test the spine first: cut a short run of the flex pattern on scrap and see whether it bends without cracking.
- 02Cut the four walls, the pin and the long cover, checking that the 612.4 mm cover fits your bed in one piece.
- 03Assemble the four walls, then wrap the cover around them, easing the flex spine into its curve before seating the joints.
- 04Glue in offcut dividers if you want sections, finish the spine with a thin oil that keeps it flexible, and fill the box.
Book on the outside, open box inside
The box itself is four walls joined at the corners. The cover is the clever part: a single 612.4 × 220 mm panel with a band of fine parallel cuts across it. Those cuts let the plywood bend into a rounded spine, so the cover wraps around the box and lies over the top like the board of a hardback. In the photo it is swung open to the left, showing the ribbed curve of the spine.
The flex spine bends best in good-quality birch plywood with no voids in the core; cheap poplar ply tends to crack along the kerf lines. Bend it slowly the first time.
Adding your own compartments
The file has one open compartment. The photo shows it organised further: a wide left section of zip pouches with peppercorns, chili and herbs, and a right section with nine small jars in three rows of three. To copy that, cut strips a little lower than the 97 mm walls from the plywood offcuts and glue them in as dividers, or leave the box open for big jars and bulk pouches.
Cutting time and bed size
Most of the work is in the spine lines: the 3 mm version has nearly 20 m of cut path. For the 3 mm file that means about 66 min 35 s on a 10 W diode, about 27 min 44 s on a 40 W CO2 and about 13 min 19 s on a 100 W CO2. The 3 mm layout is 1661 × 228 mm. The cover alone is 612.4 mm long and must be cut in one piece, while the walls can go on other sheets. A diode copes with 3 mm in one or two passes; thicker sheet makes a stiffer spine.
On a kitchen shelf it passes for a cookbook. Engrave a title on the cover with your own engrave layer and give it as a homemade spice book.
Questions about this file
Why did my flex spine crack?
Usually the plywood has voids or a brittle core. Use void-free birch plywood and bend it slowly the first few times.
Does it come with dividers?
No, inside it is a single open space. Glue in strips cut from offcuts to make sections like the jar rows in the photo.
Is 6 mm plywood a good idea for the spine?
A 6 mm version is included, but the spine is much stiffer in thick plywood, so 3 or 4 mm bends more easily and is the safer choice for a first build.
Will lacquer stop the spine bending?
A thick, hard lacquer can crack in the kerf lines. Use a thin penetrating oil or wax on the spine and lacquer elsewhere if you like.
Can I engrave a title on the cover?
Yes, the front of the cover is a large flat area. Add a title or a spice illustration as your own engrave layer.