Circle Pattern Panel SVG, Decorative Lattice Screen DXF, Room Divider Laser Cut File, Garden Fence Panel
A decorative panel pattern made of large round holes separated by small X-shaped crossbars, drawn as two identical narrow panels side by side. The free download is one SVG and one DXF file, cut lines only, with the whole layout 242.5 × 242.5 mm (9.55 × 9.55 in) and scalable to full panel size.
- Formats
- SVG, DXF
- Size
- 243 × 243 mm (9.55 × 9.55 in)
- Material
- Plywood, MDF, acrylic or metal (scale to your piece)
- Cut length
- 12.88 m
- Est. time, 10 W diode (3 mm)
- 42 min 56 s
- Est. time, 40 W CO2 (3 mm)
- 17 min 53 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Scale one panel to the height and width you need and check the crossbars are wide enough for your material.
- 02Cut the panels with plasma, router or laser and deburr the inside edges.
- 03Sand or grind the edges, then prime and paint or oil.
- 04Fix to a frame or feet and stand it or mount it on a wall.
The pattern
Large round openings alternate with small squares crossed by two curved bars, in a staggered grid, so each circle touches four crossbars. The frame around each panel is solid. The file shows two identical panels in one layout, each about half the width of the sheet and four times as tall as it is wide, which is the shape of the tall screen in the photo.
Where to use it
It works as a room divider, a privacy screen, a radiator cover front, a balcony or fence panel, a cupboard door insert or a wall panel. The photo shows a tall standing metal-style screen on small feet, painted dark blue.
Material and scaling
Plasma cut or waterjet steel and aluminium suit this design for outdoor screens, and a CNC router works well for 12 to 18 mm MDF or plywood. For a laser, scale to a smaller decorative panel. The thin crossbars are the weak point: keep them at least as wide as the material is thick, and do not scale the file down much. When you enlarge it, the bars become stronger, so large screens are easy.
Finishing
Paint or powder coat metal, and seal wood well. To make a larger divider, join several panels in a frame; repeat the pattern edge to edge, since the border lines match.
Questions about this file
Are there two panels in the file?
Yes, two identical panels sit side by side; use one or both.
Can I join panels together?
Yes, place them edge to edge on a frame to build a longer screen.
Which material suits it?
Steel for outdoors, MDF or plywood for indoors; acrylic for small decor.
How thin can the bars go?
Keep them at least as wide as the material thickness to avoid breaks.
Is it good as a room divider?
Yes, it blocks view partly and lets light through; add feet for standing.
Similar files