Tulip Silhouette DXF, Tulip Stem Cutout SVG, Spring Flower Laser Cut Blank, Wooden Tulip Wall Decor
A solid tulip silhouette with a three-petal head, a long straight stem and two upturned leaves halfway down, cut as one closed outline with no inner openings. The free download is one SVG and one DXF file with cut lines only, sized 111.8 × 223.5 mm (4.40 × 8.80 in), and it scales freely for laser or CNC cutting.
- Formats
- SVG, DXF
- Size
- 112 × 224 mm (4.40 × 8.80 in)
- Material
- Plywood, MDF, acrylic or metal (scale to your piece)
- Cut length
- 0.99 m
- Est. time, 10 W diode (3 mm)
- 3 min 17 s
- Est. time, 40 W CO2 (3 mm)
- 1 min 22 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Resize the tulip and widen the stem a little if you go much smaller than the drawn size.
- 02Cut the single outline from plywood, MDF or acrylic.
- 03Sand the petal tips and leaf edges smooth.
- 04Paint the head and leaves in two colours, then hang it or stand it in a slotted base.
The shape
This is a folk-style tulip reduced to its plainest form: a cup-shaped flower with three pointed petals, a straight stem and a pair of leaves curving up and out from the stem. It is one solid piece with a flat bottom end on the stem. The outline is hand drawn, so the petals are not perfectly symmetrical; if you prefer a crisp, even look, mirror one half in your software before cutting. The photo shows it enlarged and painted black, hung flat on a wall.
Scaling and material
At 111.8 × 223.5 mm it is a nice size for a shelf sitter or a craft blank. The stem is the narrowest part, so in thin plywood keep the flower at least this big, or widen the stem slightly when you shrink it for tags. Enlarged to 600 mm or more it becomes a wall piece; cut it from 6 mm plywood or MDF on a laser, or from 12 mm board on a CNC router so it can stand on its own in a slot base.
Spring craft ideas
Cut a row of tulips at slightly different heights and stand them in a long wooden planter box for an Easter or Mother's Day table. Painted in red, yellow and pink they make a cheerful door hanger set; left natural, they are good blanks for kids' craft sessions or painting parties. Small copies with a hole in the stem work as gift tags or garland pieces strung on twine.
Questions about this file
Does it have any cut-outs inside?
No, it is one solid outline, so the whole face can be painted or engraved.
Why are the petals a bit uneven?
The outline is hand drawn. Mirror one half in your software if you want an exactly symmetrical flower.
Can I make a tulip garland?
Yes, shrink it to about 80 mm tall, add a small hole near the top of the flower and string several on twine.
How do I make it stand up?
Cut it from thick board and push the stem end into a slot in a small block, or cut a matching slotted base from the same sheet.
What paint works on MDF?
Seal the edges with primer first, since MDF edges soak up paint, then use acrylic craft paint or spray paint.
Similar files