VisualizationLong Hair Accessory Organizer SVG, Dresser Top Hair Clip and Headband Box, Laser Cut Wooden Tray DXF
A long plywood organizer for hair accessories, 420 × 180 × 80 mm (16.54 × 7.09 × 3.15 in), with six sections: a scrunchie bay on the left, four small clip pockets in the center and a headband bay on the right, and a 40 mm front. It downloads free as SVG and DXF files for 3, 4, 5 and 6 mm plywood, and its 10 parts assemble with tabs and slots.
- Formats
- SVG, DXF
- Outer size (W × D × H)
- 420 × 180 × 80 mm (16.54 × 7.09 × 3.15 in)
- Parts
- 10
- Material thickness
- 3, 4, 5 or 6 mm plywood (a file for each)
- Layout size (3 mm file)
- 1,644 × 272 mm
- Cut length
- 7.14 m
- Est. time, 10 W diode (3 mm)
- 23 min 48 s
- Est. time, 40 W CO2 (3 mm)
- 9 min 55 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Check that your laser bed can take 420 mm parts, pick the file for your plywood and cut a test slot on scrap.
- 02Cut the 10 parts over two or three sheets, keeping the 420 mm base, front and back whole.
- 03Assemble base, sides and back, add the two long dividers, the center cross divider and its two short dividers, then the front.
- 04Sand, finish with oil or lacquer and fill the scrunchie bay, the four clip pockets and the headband bay.
A long dresser-top layout
At 420 mm this is the longest box in the hair range, yet only 180 mm deep, so it fits along the back of a dresser or vanity without taking much space. Two long dividers create three zones. The left bay holds scrunchies. The center zone is split by a cross divider and two short dividers into four small pockets, two at the back and two in front, for a matte claw clip, bobby pins, a small pink clip and a tortoiseshell clip. The right bay is wide enough for two headbands with a comb laid in front.
The front is 40 mm high and the sides rise to 80 mm, so the four center pockets stay visible from a standing height.
Cutting a long layout
The parts make a 1644 mm long layout, the longest in the set, so splitting is a must on almost any hobby machine. The base, front and back are 420 mm long: check that your bed can take that length at all before you start (a 400 mm bed cannot). For the 3 mm file, expect about 23 min 48 s on a 10 W diode, about 9 min 55 s on a 40 W CO2 and about 4 min 46 s on a 100 W CO2. Diode users should stay with 3 or 4 mm; thicker sheets suit a CO2 tube.
Assembly order: base, sides, back, the two long dividers, the center cross divider, the short back and front pockets dividers, then the front. Glue along the base helps keep a long box from bowing.
Listing and gift ideas
- A dresser-top organizer listed with "long" and the size in the title, since buyers search by length.
- A set with a matching jewellery tray in the same green-wall, warm-wood styling as the photo.
- A gift filled with six accessories, one per section.
Questions about this file
Does my laser need a long bed for this?
Yes, the base, front and back are 420 mm long. Machines with a smaller working area cannot cut them without editing the design.
What goes in the four center pockets?
Claw clips, bobby pins and small hair ties. Each pocket fits one medium claw clip.
Can I shorten it to fit a smaller laser?
You can shorten the long parts and the dividers in a vector editor. Keep all slots equal to your plywood thickness.
How do I stop a long box from bowing?
Glue the base tabs and use 4 mm plywood or thicker. A finish applied evenly on both sides of the base also helps.
Will padded headbands fit in the right bay?
Yes, the right bay is the widest section and holds two padded headbands with a comb laid in front.