Desk Name Plate SVG, Butterfly Name Holder Laser Cut File, Office Sign Panel DXF, Wooden Reception Nameplate
A flat desk name plate panel with rounded corners, a wide rectangular window across the upper half, a detailed butterfly overlapping the top edge and a small notch on each side near the middle. The free SVG and DXF contain cut lines only, in one piece measuring 228.6 × 200.7 mm (9 × 7.90 in).
- Formats
- SVG, DXF
- Size
- 229 × 201 mm (9.00 × 7.90 in)
- Material
- Plywood, MDF, acrylic or metal (scale to your piece)
- Cut length
- 2.19 m
- Est. time, 10 W diode (3 mm)
- 7 min 18 s
- Est. time, 40 W CO2 (3 mm)
- 3 min 02 s
- Layers
- CUT only, no engraving
Free account required to download
How to make it
- 01Place your name text as engraving in the lower half of the panel in your software.
- 02Cut the panel from 3 mm plywood or acrylic with engraving first.
- 03Sand the edges and the butterfly wings gently, then paint or finish.
- 04Make a base or feet to fit the side notches, or use a ready-made holder.
What it is
A single flat panel meant to stand on a desk or counter. A wide window opens the upper half, and a butterfly with open wings and slit veins sits across the top-left edge of the window. The lower half is solid and large enough for a name, a title or a company line. Two small notches on the sides, partway down, are there for a base or a bracket. The photo shows it in white painted board standing on a table.
Using it
Engrave or paint the name on the lower area, or slide a printed card behind the window. Use it at a reception, on a teacher's desk, at a salon or as a place card for a wedding table. For standing, add feet that fit the side notches or a simple slotted base. The file shows only the panel and notches, so you design the base for your material thickness.
Cutting tips
The butterfly has thin veins and a delicate antenna. Cut it from 3 mm birch plywood or acrylic and do not scale below about 180 mm wide. The window is large, so the top bar is a bit narrow; handle the panel carefully when you lift it from the bed.
Finishing
Paint it white for a clean look, or stain it. Engrave the name before cutting the outline, so it lines up. A clear coat keeps fingerprints off the wood.
Questions about this file
Is the base included?
No. The file is one panel with side notches. Make feet to match your material thickness.
Where does the name go?
The solid lower half is the name area. You can also slide a printed card behind the window.
Can I scale it?
Yes, but keep the butterfly at least 180 mm wide so the veins do not snap.
What material works best?
3 mm birch plywood or white acrylic. MDF works but can chip on the butterfly.
Can I use it as a door sign?
Yes, drill two holes at the top corners and hang it on the door.